Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T7300EG10 LS BK23346 - PA*-GF50 - BASF

Material Data Center offers the following functions for Ultramid® T7300EG10 LS BK23346:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
玻纤增强、耐热老化、可激光打标的注塑级产品,基于含芳香族成分的半结晶聚酰胺。特点是即使在吸湿后仍具有极高的强度和刚性。

市场与应用:
汽车:结构组件,金属取代,刹车部件,内饰,动力总成
电子电气:电器,手机
消费品:家用电器,消费电子,家具配件
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 7 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 5 / * kg -
模塑收缩率, 平行 0.5 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.7 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 17700 / 16600 MPa ISO 527
断裂应力 255 / 210 MPa ISO 527
断裂伸长率 2.8 / 3 % ISO 527
无缺口简支梁冲击强度, +23°C 108 / 100 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 90 / 88 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 15 / 15 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 14 / 14 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 255 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 240 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 255 / * °C ISO 75-1/-2
其它性能干 / 已调节单位Test Standard
吸湿性 1.2 / * % 类似ISO 62
密度 1600 / - kg/m³ ISO 1183
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数 134 / * cm³/g ISO 307, 1157, 1628
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 310 °C ISO 294
注塑, 模具温度 100 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 110 °C -
预干燥-时间 8 h -
加工湿度 ≤0.15 % -
注塑熔体温度 300 - 320 °C -
模具温度 80 - 120 °C -
最大停留时间 5 min -
函数
粘度-剪切速度 , Ultramid® T7300EG10 LS BK23346, PA*-GF50, BASF
剪切应力-剪切速度 , Ultramid® T7300EG10 LS BK23346, PA*-GF50, BASF
应力-应变.  , Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
应力-应变.  , Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
正割模量-应变.  , Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
正割模量-应变.  , Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
应力-应变(等时的) 23°C, Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
蠕变模量-时间. 23°C, Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
蠕变曲线 23°C, Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
应力-应变(等时的) 80°C, Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
蠕变模量-时间. 80°C, Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
蠕变曲线 80°C, Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
拉伸模量-温度 , Ultramid® T7300EG10 LS BK23346 (烘干), PA*-GF50, BASF
拉伸模量-温度 , Ultramid® T7300EG10 LS BK23346 (状况), PA*-GF50, BASF
典型数据
加工方法
注塑
供货形式
粒料, 黑色
特殊性能
经热稳处理的/耐热的
特征
可镭射打标
应用
汽车, 电子电气
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 110 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 280 - 310 °C
injection molding, Melt temperature, recommended: 300 °C
injection molding, Mold temperature, range: 80 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 5 min
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.